Posted in

What is the stress relaxation of NBR O Ring?

Hey there, let’s cut to the chase—if you work with NBR O Rings, you’ve probably heard folks toss around “stress relaxation” like it’s some niche lab term. But guess what? It’s the single most important thing that determines whether your O Ring seal holds or fails faster than a cheap disposable mask in a rainstorm. I’ve been supplying NBR O Rings for over 12 years, and I’ve lost count of how many clients have called me panicking because a seal that was perfect on day three turned into a leaky mess by day 30. 9 times out of 10, stress relaxation is the culprit, not a bad batch of O Ring. NBR O Ring

First, let’s get super simple about what it actually is—no boring textbook jargon. When you cram an NBR O Ring into a groove, you’re stretching it or compressing it (usually compression, right? Because that’s how static seals work). Stress is just that force the O Ring exerts to stay stretched/compressed, keeping two surfaces pressed tight to stop fluid or gas from escaping. Stress relaxation is what happens when that force fades over time, even if the O Ring is still sitting in that exact same spot, no one’s touched it, the temperature hasn’t spiked, nothing’s changed. It’s like how a rubber band left stretched for a week won’t snap back all the way when you let go—only with O Rings, that loss of tension is what creates gaps, leading to leaks.

Wait, why is NBR specifically prone to this? Let’s talk material science without the headache. NBR is acrylonitrile butadiene rubber, basically. The acrylonitrile (AN) content is the main variable here—higher AN means better oil resistance, but guess what? It also makes stress relaxation way worse. That’s the tradeoff every client I work with has to weigh: do you need an O Ring that won’t dissolve in diesel or hydraulic fluid, or do you need one that’ll hold its seal long-term in a static application? A 70 AN NBR O Ring is great for fuel systems, but if it’s sitting unused in a valve cover for 6 months, it’s gonna relax faster than a college student during summer break. Lower AN grades (like 40 or 50) are more flexible, hold tension way better, but they’ll go soft and turn mushy if you throw them in a gearbox with heavy gear oil. I always make sure to ask clients that exact tradeoff question before quoting, because picking the wrong AN level is the #1 mistake leading to stress relaxation issues.

Now, what causes stress relaxation in NBR O Rings anyway? Let’s break down the three main culprits that I see day to day, not the abstract stuff. First, molecular creep—rubber is made of long, tangled polymer chains, right? When you compress an O Ring, those chains get squished and can’t bounce back right away. Over time, they slide past each other, lose their “springy” shape, and that’s exactly when stress drops. Second, temperature—super important. NBR can handle up to around 250°F (120°C) for short stints, but if you leave it at 180°F for months, those polymer chains get all wobbly, slide way easier, and relaxation speeds up like crazy. I once had a construction client call me saying their NBR O Rings in a bulldozer hydraulic line failed after 8 weeks in the Arizona sun—turns out the line was sitting in engine bay heat at 190°F 24/7, way above the rating for their O Ring grade. Third, surface compression set—wait, is that the same as stress relaxation? Kind of, but not exactly. Compression set is when the O Ring never fully bounces back even after you take it out of the groove, while stress relaxation is the gradual loss of sealing force while it’s still installed. But they’re linked—too much relaxation leads to way higher compression set, and vice versa. I explain that to clients like, “If your O Ring’s tension drops 20% in 6 months, you’re looking at almost 50% compression set by year two, which is a full-on replacement job you didn’t plan for.”

Let’s give a real example to make this concrete. Last year, a guy who runs a small manufacturing shop hit me up because his new assembly line was leaking hydraulic fluid left and right. He was buying cheap, low-cost 70 AN NBR O Rings from a random supplier online, priced at $0.12 each, way cheaper than my usual $0.38. The problem? His line runs 24/7 at 160°F, and after just 90 days, those O Rings had lost 35% of their sealing force. I swapped him for a 70 AN NBR compound we specially modify to have better relaxation resistance—we tweak the curing process so the polymer chains stay tangled tight, not loose and wobbly. Those O Rings have now been running for 11 months with zero leaks, and he pays a tiny bit more, but no downtime, no emergency parts runs at 2 a.m. That’s the thing with stress relaxation—most cheap O Ring suppliers cut corners to lower cost, using subpar compounds that relax way faster. I’ve turned away 2 clients in the last year because they demanded dirt-cheap O Rings even after I warned them about relaxation issues. I’d rather lose a sale than have a client come back mad at me because their whole line is down.

Wait, can you prevent stress relaxation in NBR O Rings? 100%—it’s not some unavoidable flaw. The tricks I use with every client are the same ones I’ve refined over years of supplying parts: first, pick the right AN grade. If it’s a static seal that only sees mild temps (under 120°F) and light pressure, a 50 AN NBR will hold tension for 5+ years, no problem. If it’s a dynamic seal that moves, or needs oil resistance, go 60 AN max if you care about long life, not 70. Second, optimize the groove size. So many clients put O Rings into grooves that are too shallow, which crushes the O Ring too much—more compression = way faster stress relaxation. I always send a custom groove dimension sheet free of charge to any client, no fine print, because I’d rather get a follow-up order than hear their O Rings failed. Third, if you can, add a backup ring for extreme temps or high pressure. We make backup rings out of PTFE, which stops the NBR O Ring from getting over-compressed, slowing relaxation down by 40% or more. Fourth, curing time and compound additives—this is the stuff that separates us from random online suppliers. We cure our NBR O Rings for 2 hours at 180°C, not 45 minutes like the cheap guys, which lets the polymer chains set properly so they don’t slide over time. We also add a small amount of anti-aging and anti-relaxation additives, not just basic carbon black to make them black. I don’t brag about that publicly, but it’s why my O Rings last 2-3 times longer than the cheap ones.

Wait, what about testing? How do you know if an NBR O Ring has good stress relaxation before installing it? A lot of clients don’t have lab equipment, so I tell them a quick at-home test. Grab a sample O Ring, compress it to its installed size, weigh it down with a 5lb weight, leave it for 72 hours, then take the weight off and measure how much it bounces back. If it rebounds more than 80% of its original size, that’s good—less than 60% is garbage, will relax fast. For more formal testing, it’s standard in the industry to test stress relaxation at a fixed temperature (usually 100°C) over 70 hours, and a good NBR O Ring will lose less than 15% of its tension in that time. If you see a number over 25%, that’s a bad compound, no question. I send all my clients that test data for every batch, because I don’t hide behind my parts—if you order from me, you get the actual test results, not a generic spec sheet.

Let’s talk common myths, because I hear these all the time. Myth #1: “NBR is garbage for long seals.” No, it’s just that the wrong NBR is garbage. I have clients who use our NBR O Rings for static seals in water pump housings that have lasted 7+ years, no leaks. Myth #2: “Temperature is the only thing that causes relaxation.” Nope, like I said earlier, compression level, AN content, curing, even how the O Ring is stored. If you stack O Rings in a pile for 6 months without any space between them, the ones at the bottom get compressed from their own weight, leading to pre-relaxation before you even install them. That’s another trick I give clients—store O Rings flat, not stacked, in a cool, dry place, away from direct sunlight. Sunlight (UV rays) breaks down polymer chains, same as high temp, speeding up relaxation. Myth #3: “All O Ring suppliers use the same compounds.” Come on, I’ve tested O Rings from 5 different suppliers for the same spec, same size, same AN level, and the relaxation after 70 hours at 100°C ranged from 12% to 38%. That’s a huge difference, and it’s all about how the compound is made, how long it’s cured, what additives they use. I don’t cut corners on that, and that’s why my repeat order rate is over 80%—clients know they can count on my O Rings to hold.

Let’s circle back to why this matters to you, whether you’re a mechanic, a manufacturing owner, a heavy equipment operator, anyone. A leaky O Ring isn’t just an annoyance. If it’s a hydraulic O Ring, that’s fluid waste, downtime, lost productivity. If it’s a fuel O Ring, that’s a safety hazard, not to mention costly spills. If it’s a plumbing O Ring, that’s water damage to your building. Stress relaxation is the root cause of almost all preventable O Ring failures. I’ve seen a $10,000 per day assembly line shut down for 3 days because someone bought cheap O Rings that relaxed in 3 months, costing way more than the difference between a $0.12 O Ring and a $0.40 O Ring. That’s the math every client needs to do.

Here’s the thing: I’ve been in this game long enough that I don’t just sell O Rings—I solve problems. If you’re not sure what NBR O Ring you need, or if you’re dealing with leaky seals because of stress relaxation, just reach out. I don’t pressure you to buy a huge bulk order upfront, no fine print, no hidden fees. I’ll answer your questions, send you test data, help you pick the right compound, whatever you need. Stress relaxation doesn’t have to be a scary, confusing thing—you just need the right O Ring supplier to walk you through it.

EPDM O Ring References:

  1. Rodgers, M. (2018). Rubber Elastomers for Sealing Applications. Society of Tribologists and Lubrication Engineers.
  2. Bartenev, G. M., & Tager, A. A. (1968). Stress Relaxation in Crosslinked Rubbers. Journal of Polymer Science: Part A-2, 6(10), 1507-1521.
  3. O-Ring Handbook. (2021). Parker Hannifin Corporation, Seals Division.
  4. Lian, G., et al. (2020). Effect of Acrylonitrile Content on Stress Relaxation Behavior of NBR Elastomers. Polymer Testing, 89, 106652.

Haining Chaoyue Seals Co., Ltd.
As one of the most professional nbr o ring manufacturers and suppliers in China, we offer a wide range of products with superior quality. Please feel free to wholesale high quality nbr o ring made in China here from our factory. Also, custom service is available.
Address: Building 9, 158 Lianhong Road, Yuanhua Town, Jiaxing, Zhejiang, China.
E-mail: chaoyue@cyseals.com
WebSite: https://www.hncyseal.com/